Case Studies
30–40% Undercut Rate on 200mm+ Pipes Eliminated...
Manual TIG left 30–40% of large-diameter joints defective. Open-head orbital welding cut cycle times 60–70% and hit EN 13480 on every pass.
30–40% Undercut Rate on 200mm+ Pipes Eliminated...
Manual TIG left 30–40% of large-diameter joints defective. Open-head orbital welding cut cycle times 60–70% and hit EN 13480 on every pass.
25 mm to 150 mm OD Carbon Steel Pipe Welding at...
A Kazan construction project needed orbital welding across a 6:1 diameter ratio at 40 m elevation. Here's how one system handled it.
25 mm to 150 mm OD Carbon Steel Pipe Welding at...
A Kazan construction project needed orbital welding across a 6:1 diameter ratio at 40 m elevation. Here's how one system handled it.
16–67 mm OD Stainless Tube Welding With Zero Ch...
A Russian manufacturer needed repeatable orbital welds across 16–67 mm OD 316L tubes. One closed-head system, zero changeover, delivered in 24 days.
16–67 mm OD Stainless Tube Welding With Zero Ch...
A Russian manufacturer needed repeatable orbital welds across 16–67 mm OD 316L tubes. One closed-head system, zero changeover, delivered in 24 days.
From Radiographic Failures to PED 2014/68/EU Co...
A Polish contractor failing radiographic inspection on heat exchanger tube bundles cut weld time 65% and unlocked pharma-grade traceability with orbital automation.
From Radiographic Failures to PED 2014/68/EU Co...
A Polish contractor failing radiographic inspection on heat exchanger tube bundles cut weld time 65% and unlocked pharma-grade traceability with orbital automation.
8–15% Manual TIG Reject Rate on 1.6 mm Brewery ...
Manual TIG hits 8–15% rejects on thin-wall sanitary tube. See how closed-head orbital welding satisfies AWS D18.1 and 3-A on 316L brewery piping.
8–15% Manual TIG Reject Rate on 1.6 mm Brewery ...
Manual TIG hits 8–15% rejects on thin-wall sanitary tube. See how closed-head orbital welding satisfies AWS D18.1 and 3-A on 316L brewery piping.
From 10%+ RT Rejects to Under 2%: How a Brazili...
Manual TIG on 1-inch stainless tubes was killing shutdown margins. Mechanized orbital welding cut rejects below 2% and cycle time by 60%.
From 10%+ RT Rejects to Under 2%: How a Brazili...
Manual TIG on 1-inch stainless tubes was killing shutdown margins. Mechanized orbital welding cut rejects below 2% and cycle time by 60%.