Open-Type Orbital Welding on DN15–DN250 Fire Su...

Thin-wall fire pipe near ceilings, 200 PSI hydrostatic test, 200 joints. How an open-type orbital welder solved both without repositioning.

Open-Type Orbital Welding on DN15–DN250 Fire Su...

Thin-wall fire pipe near ceilings, 200 PSI hydrostatic test, 200 joints. How an open-type orbital welder solved both without repositioning.

304/316L sanitary piping in Western Canada fall...

304/316L sanitary piping in Western Canada falls under ASME BPE and 3-A Sanitary Standards, both of which mandate full-penetration root passes with smooth internal bead profiles — criteria that manual...

304/316L sanitary piping in Western Canada fall...

304/316L sanitary piping in Western Canada falls under ASME BPE and 3-A Sanitary Standards, both of which mandate full-penetration root passes with smooth internal bead profiles — criteria that manual...

8–12% Rework to Under 2%: Copper Tube Welding f...

An Indian refrigeration OEM slashed brazed-joint rework from 8–12% to under 2% by switching to orbital tube welding. Here's what changed.

8–12% Rework to Under 2%: Copper Tube Welding f...

An Indian refrigeration OEM slashed brazed-joint rework from 8–12% to under 2% by switching to orbital tube welding. Here's what changed.

From 15% Leak Rate to Under 2%: How an Indian R...

An Indian refrigeration OEM cut joint rework from 15% to under 2% and tripled shift output by replacing manual torch brazing with automated tube welding.

From 15% Leak Rate to Under 2%: How an Indian R...

An Indian refrigeration OEM cut joint rework from 15% to under 2% and tripled shift output by replacing manual torch brazing with automated tube welding.

From 15–20% Weld Rejection to Under 2%: Open-He...

Field retrofit piping in Bolivia cut weld rejection from ~18% to under 2% using open-head orbital welding on Sch-40 stainless and carbon steel up to 4".

From 15–20% Weld Rejection to Under 2%: Open-He...

Field retrofit piping in Bolivia cut weld rejection from ~18% to under 2% using open-head orbital welding on Sch-40 stainless and carbon steel up to 4".

Tube-to-Tubesheet Orbital Welding for HVAC Heat...

HVAC heat exchanger fab cut joint cycle time 50–60% and hit >95% first-pass X-ray rate using orbital tube-to-tubesheet welding. Full process breakdown.

Tube-to-Tubesheet Orbital Welding for HVAC Heat...