8–15% X-Ray Rejection to Under 2%: How a Colomb...
A Colombian oil & gas contractor cut stainless steel weld rejection from 15% to under 2% and unlocked refinery turnaround contracts using orbital welding.
8–15% X-Ray Rejection to Under 2%: How a Colomb...
A Colombian oil & gas contractor cut stainless steel weld rejection from 15% to under 2% and unlocked refinery turnaround contracts using orbital welding.
Open-Type Orbital Welding on DN15–DN250 Fire Su...
Thin-wall fire pipe near ceilings, 200 PSI hydrostatic test, 200 joints. How an open-type orbital welder solved both without repositioning.
Open-Type Orbital Welding on DN15–DN250 Fire Su...
Thin-wall fire pipe near ceilings, 200 PSI hydrostatic test, 200 joints. How an open-type orbital welder solved both without repositioning.
304/316L sanitary piping in Western Canada fall...
304/316L sanitary piping in Western Canada falls under ASME BPE and 3-A Sanitary Standards, both of which mandate full-penetration root passes with smooth internal bead profiles — criteria that manual...
304/316L sanitary piping in Western Canada fall...
304/316L sanitary piping in Western Canada falls under ASME BPE and 3-A Sanitary Standards, both of which mandate full-penetration root passes with smooth internal bead profiles — criteria that manual...
8–12% Rework to Under 2%: Copper Tube Welding f...
An Indian refrigeration OEM slashed brazed-joint rework from 8–12% to under 2% by switching to orbital tube welding. Here's what changed.
8–12% Rework to Under 2%: Copper Tube Welding f...
An Indian refrigeration OEM slashed brazed-joint rework from 8–12% to under 2% by switching to orbital tube welding. Here's what changed.
From 15% Leak Rate to Under 2%: How an Indian R...
An Indian refrigeration OEM cut joint rework from 15% to under 2% and tripled shift output by replacing manual torch brazing with automated tube welding.
From 15% Leak Rate to Under 2%: How an Indian R...
An Indian refrigeration OEM cut joint rework from 15% to under 2% and tripled shift output by replacing manual torch brazing with automated tube welding.
From 15–20% Weld Rejection to Under 2%: Open-He...
Field retrofit piping in Bolivia cut weld rejection from ~18% to under 2% using open-head orbital welding on Sch-40 stainless and carbon steel up to 4".
From 15–20% Weld Rejection to Under 2%: Open-He...